Air-release PVC · removable grey adhesive · matte laminate
Self-adhesive graphics for equipment installed by an operator in a car park, not by a wrapper in a bay: air-release film, removable adhesive, matte laminate, cut to the panel.
A battery swap cabinet is a flat steel box with panel seams, screw recesses, a vent slot and a hinge. The graphic goes on at a kerbside by an operations technician with a squeegee and, if the day is going well, a felt edge. Nothing in that job needs a film that stretches 130 %. It needs a film that goes down without trapping air, and comes off in eighteen months without taking the powder coat with it.
The failure we see most is not fading. It is edge lift after the second summer, and adhesive transfer when the operator pulls a campaign panel off a machine that has been sitting at 65 °C in the sun. So this page is specified around the removal rather than the application: an air-release channel in the adhesive, removable grey at 12–15 N/25 mm, and a matte laminate that stops the cabinet face mirroring the LED panel opposite.


Air-release PVC · removable grey adhesive · matte laminate

Die-cut one decal per door · S / M / L door map · numbered

140 gsm outdoor PVC · opaque on black · matte or anti-scratch

Low-tack 5–8 N/25 mm · swaps quarterly · no residue


Cast film · 5 yr outdoor · contour cut · reflective option

Colour-white-colour · blocks a dark substrate

0.3 mm rigid label stock · permanent high-tack · die-cut

Pictograms + QR + serial · anti-scratch · kiss-cut sheet

Resists IPA & disinfectant · wipe-clean face

Cast PVC 50 µm · LSE adhesive · cut around antennas and vents
Send the cabinet outline as a 1:10 PDF with every panel on its own layer, plus the door swing and vent positions marked. We split the artwork on the seams you draw and leave a 2 mm gap so the film cannot bridge the joint. Cut path on a spot-colour layer named CUT.
Rolled print-side out, one roll per cabinet, labelled with cabinet model and site code. A printed panel map goes inside the tube so the technician knows which sheet goes where without calling you.
Sample 2–3 wd · 50 cabinets 6–8 wd · sea 18–28 d
Give us the bank elevation with every door dimensioned and a numbering scheme (A1, A2, B1 …). One artboard per door size, not per door, unless the graphics differ. We generate the numbering from your map and send a proof sheet before cutting.
Bundles in door order, wrapped in paper, each bundle labelled with the door range it covers. Loose singles are packed in the same sequence as the map so a two-person install does not need to sort.
Sample 3–4 wd · 30 banks 7–9 wd · sea 18–28 d
Mask the glass, the coin mechanism and the delivery flap in the file — do not leave them to be trimmed on site. Send a photo of the machine alongside the artwork if you have one; the panel gaps on a vending cabinet are rarely where the drawing says they are.
Rolled per machine with a fitting sheet showing the panel sequence. Glass and mech cut-outs are marked on the backing paper so the installer can line up before peeling.
Sample 2–3 wd · 50 machines 6–8 wd · sea 18–28 d
Same panel outline as the permanent version, so one artwork template serves both. Keep critical logos 30 mm inside the panel edge — a removable panel is handled more, and the edge is where it lifts first.
Flat-packed between boards rather than rolled, because a low-tack film takes a set in a tight roll and then will not lie flat on a door.
Sample 2–3 wd · bulk 4–6 wd · sea 18–28 d
A 3D shell does not flatten cleanly. Send the shell as a flat pattern if the industrial designer has one, otherwise send the STEP file and we will flatten it and send back a PDF pattern for approval before print.
Flat in a rigid envelope, one bag per unit, so a set stays together. Small decals are kiss-cut on a sheet with the unit number printed in the margin.
Sample 3–4 wd · 200 units 6–9 wd · air 5–8 d
Fleet work needs a colour target, not a screen. Send a Pantone reference for the brand colour and we will send a printed swatch on the actual film before the run — a green that looks right on an iMac is often two shades off on cast vinyl.
Rolled per unit with a panel sequence sheet. Registration marks are printed on the liner, not the face, so nothing has to be wiped off before fitting.
Sample 3–4 wd · 50 units 7–10 wd · sea 18–28 d
Mark the white layer explicitly: a spot colour named WHITE, 100 % tint, on its own layer. If the artwork is supplied flat with no white layer we will add it and show you the difference on a proof over black.
Rolled print-side out. Because the white base makes the film stiffer, we ship it flat over 1 m and rolled under, and mark the roll “white base — do not crease”.
Sample 3–4 wd · bulk 5–7 wd · sea 18–28 d
Vector only, at final size, with the die line on a spot-colour layer named CUT. Text below 5 pt on a matte silver stock fills in on the press — if the rating data has to be legible, 6 pt is the floor.
Kiss-cut sheets of 20, banded, with the label count written on the band. Loose die-cut labels ship between two boards so the corners do not lift in transit.
Sample 3–4 wd · 5,000 labels 5–7 wd · air 5–8 d
Send the QR content as a URL and we will generate and verify the code, or send the vector code with a 10-module quiet zone. Pictograms should be vector; a lifted PNG at 300 dpi fails at label size.
Sheets banded in application order with a paper template showing where each label goes on the machine. One template per machine model.
Sample 3–4 wd · 2,000 sheets 6–8 wd · sea 18–28 d
Tell us the cleaning agent if it is aggressive — chlorine and some solvent wipes attack standard laminate and no print survives that. We will name the laminate in the quotation so the specification is on record.
Rolled print-side out with an interleaf, because a chemical-resistant laminate is softer and marks if it is rolled face-to-back.
Sample 3–4 wd · bulk 5–7 wd · sea 18–28 d
Send a dimensioned drawing of each face you want covered and mark the no-go zones: antenna covers, vent grilles, obstacle-sensor windows, GPS patch and the battery bay. A decal over an antenna is not a cosmetic mistake — it detunes the link and shows up as reduced range, not as a visible fault. Registration marks have to match the format your authority requires (Remote ID, EU class label, or the real-name QR code), so we set them at the size the rule states rather than the size that looks balanced.
One poly bag per aircraft set, pieces numbered against an A4 placement sheet, packed flat rather than rolled — a 50 µm cast film takes a curl memory that a 100 µm film never does.
Sample 3–4 wd · 200 sets 5–7 wd · air 7–10 d
| Asset | Recommended media | Adhesive | Laminate |
|---|---|---|---|
| Battery swap cabinet — campaign refreshed every 6–12 months | Air-release PVC, 100 µm | Removable grey, 12–15 N/25 mm | Matte |
| Parcel locker bank — doors handled all day | Air-release PVC, 100 µm, die-cut per door | Removable grey | Matte + anti-scratch |
| Vending machine — outdoors, full sun | Outdoor PVC, 140 gsm | Removable grey | Matte or anti-scratch |
| Fixed rating plate / warning label | Rigid PVC label stock, 0.3 mm | Permanent high-tack grey | Matte |
| Robot or AMR — curved shell, refurbished later | Cast PVC, 80 µm, air-release | Low-tack, ≤ 8 N/25 mm | Matte |
| Black cabinet — colour must stay true | Air-release PVC + white ink base | Removable grey | Matte |
| Drone or UAV — carbon-fibre shell, weight-critical | Cast PVC, 50 µm | LSE acrylic, low-tack option | Thin matte, 30 µm |
| Panel wiped with disinfectant daily | PVC, 100 µm | Permanent or removable | Chemical-resistant matte |
| Locker ad face — image changes quarterly | PVC, 100 µm, low-tack | Low-tack, 5–8 N/25 mm | Matte |
Every job is quoted with the asset written down, because “vinyl decal” on its own does not describe a product. Where the brief is unclear we ask for a photo of the cabinet and the cleaning routine before naming a film.
Four adhesives cover everything on this page, and they are not interchangeable. Low-tack is for graphics that are swapped quarterly. Removable grey is the workhorse: strong enough for a cabinet face in full sun, clean enough to peel in one piece inside two years. Permanent grey is for rating plates that are never meant to come off. High-tack exists because textured powder coat and polypropylene shells reject everything else.
The laminate is chosen by what happens to the machine, not by how it looks: matte for glare and photographs, anti-scratch for anything at grab height, chemical-resistant where the panel is wiped with 70 % IPA every shift. On a device that is disinfected daily, standard matte hazes within months — that is a laminate problem, not a print problem.

| Adhesive | Peel strength | Dwell | Best for | Residue on removal |
|---|---|---|---|---|
| Low-tack removable | 3–8 N/25 mm | 3–6 months | Campaign panels, robot shells | No, on powder coat and ABS |
| Removable grey | 12–15 N/25 mm | up to 24 months | Swap cabinets, lockers, vending | No, within the dwell window |
| Permanent grey | 18–25 N/25 mm | 5 yr + | Rating plates, warning labels | Yes — mechanical removal |
| High-tack permanent | 25 N/25 mm + | 7 yr + | Textured or low-energy shells (PP, PE) | Yes — and it takes the coat |
| Laminate | Does what | Adds | Specify when |
|---|---|---|---|
| Matte, 80 µm | Kills glare | Scuff resistance | Cabinet faces next to an LED panel, anything photographed |
| Gloss, 80 µm | Colour depth | Scuff + light UV | Dark cabinets where depth matters more than reflection |
| Anti-scratch matte | Hardest surface | Abrasion | Locker doors and panels at grab height |
| Chemical-resistant | Wipe-clean | IPA and disinfectant | Machines cleaned daily |
| Anti-graffiti | Sacrificial layer | Marker and spray | Street-level cabinets and public transport |
A device is a set of panels, not a single canvas. The artwork has to be split on the seams the manufacturer built in, or the film bridges a joint that opens every time the door is used — and a bridged joint lifts within weeks. Send the outline, mark the seams, and we will do the splitting and send back a panel map for approval.
The second thing that gets missed is the white base. On a black cabinet, colour printed without it reads olive; the proof looks right because it is on white paper. Ask for the proof on the actual film, over the actual cabinet colour, or you will find out at install.
| Item | We need | Why |
|---|---|---|
| Device outline | 1:10 PDF or DXF with panel seams | We split on your seams, not ours |
| Panel map | Every panel named and dimensioned | One roll per panel, no guessing on site |
| Door / hatch swing | Marked on the drawing | So the film never bridges a hinge |
| Vent and screw positions | On a separate layer | Cut-outs land on the recess, not beside it |
| Cut line | Layer named CUT, spot colour | Drives die-cut and kiss-cut |
| Seam gap | 2 mm at every joint | A 1 mm gap gets bridged, then lifts |
| White base | Layer named WHITE at 100 % | Dark cabinets need it or the colour shifts |
| Colour | CMYK; Pantone for the logo | Holds ΔE ≤ 2 across a fleet |
Every cabinet, locker bank or machine ships as its own roll, labelled with model and site code. Nothing on site has to be measured or cut.
A printed A4 showing which sheet goes where, in what order. The single biggest cause of a bad install is the technician inventing a sequence.
Damaged in transit, dropped on a kerb, applied crooked — a 5 % spare allowance costs less than an air-freight resend of one panel.
| Stage | Under 100 m² | 100–500 m² | Kitted rollout | Notes |
|---|---|---|---|---|
| Artwork check | same day | same day | same day | Marked-up proof or a pass, by email |
| Physical proof | 2–3 wd | 3–4 wd | 3–4 wd | Printed on the actual film, couriered |
| Production | 4–6 wd | 6–9 wd | 8–12 wd | After written proof approval |
| Die-cut & kitting | 1–2 wd | 2–3 wd | 3–4 wd | Kitted and labelled per device |
| Sea freight | 18–28 d | 18–28 d | 20–30 d | Shenzhen to EU / US, port to port |
| Air freight | 5–8 d | 5–8 d | 6–9 d | Door to door, volumetric weight |
Working days from written proof approval. A kitted rollout adds a day or two at the end for labelling and carton mapping, which is cheaper than a site that cannot match cartons to machines.
Self-adhesive vinyl with an air-release channel in the adhesive, so trapped air is pushed out with a squeegee instead of being punctured.
DefinitionWhite ink underlayerA white base printed under the colour on clear or dark media. On a black cabinet it is the difference between the colour you approved and a muddy version of it.
DefinitionKiss cutCutting the print but not the backing paper, so individual labels peel off a sheet one at a time. Every label set on this page is supplied this way.
DefinitionLaminationA protective film over the print: matte to kill glare, anti-scratch for high-touch doors, chemical-resistant for machines that are wiped daily.
DefinitionOnly if the film outlives its adhesive. Removable grey is rated for about 24 months of dwell; low-tack for three to six months. Peel a low-tack panel after three years and it comes off like a permanent one, with the residue to match. The number to write into your procurement spec is the dwell time, not the word “removable”. Peeling warm — above 15 °C, slowly, at 30° to the surface — removes cleanly inside that window.
If the print has no white base, yes. A pale colour printed straight onto black powder coat reads olive, and a mid-grey reads charcoal; this is the most common colour complaint on device work and it is entirely avoidable. We lay 100 % white first, then colour, then an optional white hit on top (colour-white-colour). Budget roughly 25 % more per m² and you get the colour you approved on screen.
The film survives; the edges are what fail. A painted steel cabinet face reaches 60–70 °C on a still sunny day, and a 100 µm film with a matte laminate and a properly cut edge holds that for three years. What kills it is a film bridged across a 1 mm panel gap or wrapped round a sharp return — both of which lift at the corner and then peel back. That is why we cut to your seams and leave a 2 mm gap.
Yes, with air-release film and a plan. Split the cabinet into panels at the seams, start at one edge, hinge the film with tape, and squeegee in one direction with 30 % overlap. The channels in the adhesive let trapped air out at the edge instead of being trapped. On a 1.9 m single sheet with no channels, one person will lose — which is why the film spec matters more than the technique.
Yes. Each device gets its own labelled roll, each carton carries a site code, and we can drop-ship to multiple addresses against one order. For rollouts above about 50 units we also print a per-site packing list and a panel map per model, so the receiving site can check the carton without opening every roll.
Some areas are off limits, and they are why a drone decal is not a small vehicle wrap. Keep film off the antenna covers, the GPS patch, vent grilles and the obstacle-sensor windows — a film with adhesive over an antenna detunes the link, and the symptom is reduced range rather than anything you can see. Nothing goes on a propeller either: even 0.2 g changes the balance. What is left — flat side panels, the arms, the outer battery door — is plenty of area for a livery, and it is the area our cut file is drawn around.